Temabond WG 200
|
|
描述 |
A two component, low temperature curing, aluminium pigmented high-solids modified epoxy paint. |
产品特性 |
Especially used as a primer for steel surfaces difficult to clean in process and chemical industry and in water immersion. Excellent adhesion to blast cleaned or hand prepared steel. Recommended for repairing of damages caused by transport or installation. Can also be applied on old alkyd paint surfaces and as a single coat paint. |
推荐用途 |
Recommended for repainting and touch-up painting of bridges, cisterns and different types of steelwork and equipment in wood-processing and chemical industry, such as paper machines, conveyors, tubular bridges etc. |
|
技术参数 |
特性 |
Good chemical, solvent and abrasion resistance, due to the aluminium pigments. High film build properties, also by brush. Low solvent content - lower solvent emissions than with traditional epoxy paints. |
色彩类别 |
Aluminium. The colour will change in outdoor use. |
光泽组别 |
半光 |
涂布率 |
Recommended film
thicknesses
|
Theoretical
coverage
|
dry
|
wet
|
|
100
µm
|
125
µm
|
8.0
m2/l
|
200
µm
|
250
µm
|
4.0
m2/l
|
Practical
coverage depends on the application method, painting conditions and the shape
and roughness of the surface to be coated.
|
混合比例 |
Base 1 part by volume 008 7510
Hardener 1 part by volume 008 7519 |
涂刷方法 |
By
airless spray or brush. |
适用期 |
1½ hours |
干燥时间 |
DFT 150 µm
|
-5 ºC
|
0 ºC
|
+ 5 ºC
|
+ 10 ºC
|
+ 23 ºC
|
Dust dry, after
|
18 h
|
14 h
|
6 h
|
3 h
|
2 h
|
Touch dry, after
|
48 h
|
36 h
|
17 h
|
9 h
|
5 h
|
Recoatable, min. after
|
48 h
|
36 h
|
17 h
|
9 h
|
5 h
|
Recoatable without sanding, max. after
|
2 months
|
2 months
|
2 months
|
1 month
|
14 d
|
Drying
and recoating times are related to the film thickness, temperature, the
relative humidity of the air and ventilation.
|
Solids volume |
80 ± 2 volume % (ISO 3233)
83 ± 2 weight % |
密度 |
1.3 kg / l (mixed) |
产品编号 |
008 7510 |
|
使用说明 |
施工条件 |
All surfaces must be dry. The temperature of the ambient air and the surface should not fall below - 5 ºC during application and drying, the temperature of the paint should be at least +15 ºC. Relative humidity should not exceed 80 %. The surface temperature of the steel should remain at least 3 ºC above the dew point. |
准备 |
Oil, grease, salts and dirt are removed by appropriate means. (ISO 12944-4)
Steel surfaces: Remove rust by tool cleaning to minimum St2 or blast clean to Sa2½ . Blast clean to grade Sa2½ for immersion. (ISO 8501-1).
Earlier painted surfaces: Roughen old paint surfaces using e.g. abrasive wheel, sand paper or blast cleaning. |
涂刷底漆 |
TEMABOND WG 200. |
喷面漆 |
TEMACOAT GPL, TEMACOAT GPL-S MIO, TEMACOAT GPL-S PRIMER, TEMACOAT GS 50, TEMACOAT RM 40, TEMADUR, TEMATHANE, TEMACRYL EA, TEMABOND WG 300 and ST 300. |
涂刷 |
By airless spray or brush. Depending on the temperature of the components the paint can be thinned 0 - 10 %. Airless spray nozzle tip 0.013" - 0.019" and nozzle pressure 120 - 180 bar. Spray angle shall be chosen according to the shape of the object. At brush application the paint should be thinned according to the circumstancies. |
成分混合 |
First stir base and hardener separately. The correct proportions of base and hardener must be mixed thoroughly before use. Use Temaspeed Squirrel Mixer for mixing. |
工具清洗 |
Thinner 1031. |
EU VOC 2004/42/EC-限值 |
The Volatile Organic Compounds amount is 220 g/litre of paint.
VOC content of the paint mixture (thinned 10 % by volume) is 280 g/l. |
|