Tikkurila worldwide
产品使用说明书
21.05.2008

Temacoat GF Primer

 
Tikkurila Industry 9L
描述 A two component, polyamide cured epoxy primer containing zinc phosphate.
产品特性 Used as a primer for steel, aluminium and zinc surfaces in epoxy and polyurethane systems, when high requirements for the appearance are set.
推荐用途 Recommended for agricultural machinery, haulage equipment and other machinery and equipment.

技术参数
色卡 Temaspeed Primers colour card. TEMASPEED tinting.
光泽组别 半哑光
涂布率

Recommended film thicknesses

Theoretical coverage

dry

wet

 

50 µm

90 µm

11.0 m2/l

70 µm

130 µm

7.8 m2/l


Practical coverage depends on the application method, painting conditions and the shape and roughness of the surface to be coated.
混合比例 Base 4 parts by volume 178-series
Hardener 1 part by volume 008 5600 or 008 5605 (fast)
涂刷方法 By airless or conventional spray or by brush.
适用期 6 hours with Hardener 008 5600
3 hours with Hardener 008 5605
干燥时间

DFT 60 µm

0 ºC

+ 5 ºC

+ 10 ºC

+ 23 ºC

+ 35 ºC

Dust dry, after

with Hardener 008 5600

4 h

2 h

1 h

½ h

15 min

with Hardener 008 5605

3 h

1½ h

¾ h

½ h

12 min

Touch dry, after

with Hardener 008 5600

22 h

11 h

5 h

2½ h

2 h

with Hardener 008 5605

12 h

6 h

3½ h

2 h

1½ h

Recoatable with epoxy paints, min. after

with Hardener 008 5600

30 h

20 h

6 h

2 h

1 h

with Hardener 008 5605

18 h

12 h

4 h

1½ h

¾ h

Recoatable with polyurethane paints, min. after

with Hardener 008 5600

2 d

32 h

18 h

6 h

3 h

with Hardener 008 5605

1 ½ d

18 h

12 h

4 h

2 h


Drying and recoating times are related to the film thickness, temperature, the relative humidity of the air and ventilation.
Solids volume 55 ± 2 % volume (ISO 3233)
70 ± 2 % weight
密度 1.4 kg / l (mixed)
产品编号 178-series

使用说明
施工条件 All surfaces must be dry. The temperature of the ambient air, surface or paint should not fall below + 5 ºC during application or drying. Relative humidity should not exceed 80 %. The surface temperature of the steel should remain at least 3 ºC above the dew point.
准备 Oil, grease, salts and dirt are removed by appropriate means. (ISO 12944-4)

Steel surfaces: Blast clean to grade Sa2½. (ISO 8501-1) If blast cleaning is not possible, phosphating is recommended for cold rolled steel to improve adhesion.

Zinc surfaces: Sweep blast clean with mineral abrasives, e.g. quartz sand, to an even roughness. (SaS, SFS 5873) If sweep blasting is not possible, the surface should be roughened by hand abrading or washed with PANSSARIPESU detergent.

Hot dip galvanized surfaces are recommended to be painted with a misty coat (paint thinned 25 - 30 %) before the actual priming.

Aluminium surfaces: Sweep blast clean with non-metallic abrasives to an even roughness. (SaS, SFS 5873) If sweep blasting is not possible, the surface should be roughened by hand abrading or washed with FONTECLEAN AL detergent.

Primed surfaces: Oil, grease, salt and dirt are removed from the surface by appropriate means. Repair any damage to the primer coat. Note the overcoating time of primer. (ISO 12944-4)
涂刷底漆 TEMACOAT GF PRIMER, TEMAZINC 77, TEMAZINC 88 and TEMAZINC 99.
喷面漆 TEMACOAT GPL, TEMACOAT GS 50, TEMACOAT RM 40, TEMACOAT GPL-S MIO, TEMADUR, TEMATHANE and TEMACRYL EA.
涂刷 By airless or conventional spray or by brush. At airless spray application the paint should be thinned 5 - 25 %. Airless spray nozzle tip 0.011" - 0.017" and nozzle pressure 120 - 180 bar. Spray angle shall be chosen according to the shape of the object. At conventional spray the paint should be thinned 20 - 30 % to a viscosity of 20 - 30 s DIN4. At brush application the paint should be thinned according to the circumstancies.
成分混合 First stir base and hardener separately. The correct proportions of base and hardener must be mixed thoroughly before use. Use Temaspeed Squirrel Mixer for mixing.
工具清洗 Thinner 1031.
EU VOC 2004/42/EC-限值 The Volatile Organic Compounds amount is 420 g/litre of paint mixture.
VOC content of paint mixture (thinned 30 % by) volume is 524 g/l.

健康安全等级
Containers are provided with safety labels, which should be observed. Further information about hazardous influences and protection are detailed in individual health and safety data sheets. A health and safety data sheet is available on request from Tikkurila Oy.
 
-


返回